Tried quenching in warm water instead of cold and the file skated right off
Last Saturday I finally heat treated a set of three 1084 camp knives I'd been sitting on since March. I usually quench in cold water from the hose, but the guy who runs the shop down in Peru told me to try warm water around 100 degrees instead, so I did. Two of the three came out hard enough that a file skated clean off, but the third warped about 1/16 inch at the tip and I had to grind it back down. Now I'm stuck arguing with myself about whether the warm water helped or if I just got lucky on two of them. The cold water batch I did in February had one soft spot, so maybe warm is better, but that warp bugs me. Anyone here run warm water on simple steels, and did you get warping too?