Swore off layout fluid on aluminum until a guy at the Rockford trade show proved me wrong
I always thought layout fluid was a waste on aluminum since it smears and stains, so I just used a sharpie and eyeballed my punch marks. Then I stood at a booth in Rockford watching a guy coat a 6061 plate with Dykem and scribe lines so crisp you could read them from four feet away. He told me the trick was letting it dry a full 15 mins before touching it, which I never did. Tried it on a bracket job the next week and my hole spacing was dead on the first try. Anyone else change their mind on marking methods after seeing it done in person?