Walked through a shop in Tulsa last week and saw a tech prepping panels with 80 grit before sealer
Stopped by a buddy's shop in Tulsa while he was finishing a silver Camry re-spray, and his prep guy was going over bare metal and filler with 80 grit before laying sealer. My gut says that's way too coarse and you'll see sand scratches pop through the base coat, but he swears the sealer fills it and he's been doing it that way for years with no comebacks. I've always finished prep at 180 or 220 before sealer, so now I'm second guessing myself. What grit are you all finishing at before sealer on a full panel?